Acrylic Finish Coating
Description:
The acrylic finish coating (acrylic paint) can only be used under the conditions that the substrate temperature is at least 3℃ higher than the dew point, and the relative humidity is less than 85%. And also it needs to remove oil, dust and other pollutants from the surface properly, or scrub it clean with the thinner for the acrylic finish coating. The acrylic finish coating (acrylic paint) can be applied to freeboard, water line, and superstructure of vessels, as well as metal structures and concrete for corrosion resistance.
Founded in 1976, Zhongbang Chemical Group Co.,Ltd is a professional manufacture and supplier of acrylic finish coating. Besides acrylic finish coating, we can also provide chlorinated rubber cover coating, heat resistant paint, acrylic coating, alkyd primer (alkyd paint), and so on. All of our products have passed the certification of ISO9001: 2000. Our products have been well received by customers from Russia, Spain, Ukraine, Holland, India, Mexico, and many countries and regions in Africa. If you need high quality acrylic finish coating and want to know more information, please contact us freely.
Instructions
Mixture Ratio | One-pot coating | |||
Curing Time | As long as the acrylic finish coating is stirred uniformly. | |||
Shelf Life | Limitless | |||
Coating Methods | Airless spraying, air spraying, manual brushing and roller coating | |||
Thinner | X-14 Chlorinated rubber paint thinner | |||
Airless Spraying | Air Spraying | Manual Brushing and Roller Coating | ||
Maximum Dilution | 5% | 10% | 3% | |
Spray Holes | 0.4~0.5mm | 2.0~3.0mm | - | |
Spraying Pressure | 15~30MPa | 0.3~0.5MPa | - | |
Tool Cleaning | X-14 Chlorinated rubber paint thinner | |||
Paint Film Thickness | Wet film: 175um, Dry film: 50um | |||
Coating Interval | Substrate Temperature | 0℃ | 20℃ | 30℃ |
The shortest interval | 24h | 8h | 6h | |
The longest interval | Limitless | |||
Preceding Coats | Chlorinated rubber aluminum powder thick slurry anti-rust paint, high build chlorinated rubber iron red antirust paint, chlorinated rubber micaceous iron oxide anti-rust paint, epoxy MIO antirust paint, etc. |
Parameters
Color | All colors |
Gloss | Semi-gloss |
Theoretical Coverage | 200g/m2 |
Specific Weight | Approximately 1.25 |
Drying Time | 23±2℃: Surface drying ≤2h, Complete drying ≤8h |
Flash Point | 25℃ |
Storage Life | 12 months |
- Chlorinated Rubber Cover CoatingThe chlorinated rubber cover coating (chlorinated rubber paint) is made of chlorinated rubber, pigments, plasticizer, additives, solvents, and more ...